Steel High Temperature Temper Brittleness

Sep 13, 2022

Leave a message

High temperature tempering brittleness: many alloy steels are tempered between 500 and 550 °C after quenching, or the embrittlement occurs when they pass through the 500 to 550 °C range with a slow cooling rate after tempering at a temperature above 600 °C. If it is reheated to a temperature above 600 °C and then rapidly cooled, the toughness can be restored, so it is also called reversible temper brittleness. It has been proved that impurity elements such as P, Sn, Sb, As in steel segregate to the prior austenite grain boundary at a temperature of 500-550 °C, resulting in high temperature temper brittleness; elements such as Ni and Mn can interact with impurity elements such as P and Sb.

Grain boundary co-segregation (cosegregation), and Cr element promotes this co-segregation, so these elements increase the high temperature temper brittleness of steel. On the contrary, the interaction of molybdenum and phosphorus hinders the segregation of phosphorus at grain boundaries, which can reduce the brittleness of high temperature tempering. Rare earth elements also have a similar effect. Rapid cooling of steel after tempering at temperatures above 600°C can inhibit the segregation of phosphorus, and is often used in heat treatment operations to avoid high temperature temper brittleness.

format,f_auto.webp