The properties of quenched steel after tempering depend on its internal microstructure; the microstructure of steel varies with its chemical composition, quenching process and tempering process. Carbon steel can obtain better mechanical properties after tempering between 100 and 250 ℃. The typical changes of mechanical properties of alloy structural steel after tempering between 200 and 700 ℃ are: with the increase of tempering temperature, the tensile strength σb of the steel decreases monotonically; the yield strength σ0.3 first increases slightly and then decreases ; Section shrinkage ψ and elongation δ are improving continuously; toughness (using fracture toughness K1c as an indicator) generally tends to increase, but there are two minimum values between 300 and 400 °C and between 500 and 550 °C.
Correspondingly, they are called low temperature temper brittleness and high temperature temper brittleness. Therefore, in order to obtain good comprehensive mechanical properties, alloy structural steels are often tempered in three different temperature ranges: ultra-high strength steels are tempered at about 200 to 300 °C; spring steels are tempered at around 460 °C; quenched and tempered steels are tempered at 550 to 650 °C. fire. Carbon and alloy tool steels are required to have high hardness and strength, and the tempering temperature generally does not exceed 200 °C. Alloy structural steel, die steel and high-speed steel with secondary hardening during tempering are all tempered in the range of 500 to 650 °C.