Stress corrosion cracking of stainless steel is not common in printing and dyeing machinery, but if there are certain corrosive components and appropriate temperature conditions, the risk of stress corrosion cracking on the surface of stainless steel will be reduced when subjected to stress or residual tensile stress. very big. One of the reasons is that the inner surface of most high-temperature equipment still has some residual internal stress after processing. If there is only tensile stress and no compressive stress, corrosion cracking will occur with the presence of stress. 

Chloride, caustic soda solution, sodium sulfate, and tap water with a certain chloride ion content are commonly used solvents in industry, and they are also common "killers" of stainless steel. A solution of sodium chloride not higher than 60°C is sufficient to induce cracks in the stressed area, while only a 20% solution of sodium hydroxide in a caustic soda solution is required at 130°C to initiate cracks.

Complete relief of tensile stress is not possible for mechanical construction, especially on pressure vessels. Therefore, in the actual operation process, it is extremely important to control the critical temperature. Eliminating or not using high-temperature printing and dyeing auxiliaries that generate chloride ions is an important measure to prevent stress corrosion cracking.

In recent years, the smelting technology of dual-phase steel has advanced by leaps and bounds, and has the same excellent anti-corrosion properties as austenite, which has been used in the printing and dyeing industry. Since dual-phase steel has higher strength and lower stress than austenite, in some environments, the application of dual-phase steel can greatly reduce the occurrence of stress corrosion. Reduce the thickness of the material used.

format,f_auto.webp