The process of pitting corrosion formation: pitting corrosion begins with metastable pitting corrosion behavior. For various defects on the surface of stainless steel, such as surface sulfide inclusions, grain boundary carbide deposition, surface grooves, etc., the passivation film is first damaged, exposing the base metal to appear small corrosion holes (the pore size is mostly 20~30μm), which is The metastable pore nucleus becomes the active center for pitting corrosion. After the nucleation is formed, a considerable part of the dots may still be passivated again.
If the resistance to repassivation is small, the nucleation will not grow. When the corrosion nuclei continue to grow to a certain critical size (generally the pore size is greater than 30 μm) under the influence of promoting factors, macroscopically visible corrosion holes appear on the metal surface, and this specific point becomes the pitting corrosion source. Once the pit is formed, the growth will be accelerated. Now, take the corrosion process of stainless steel in a gas-filled chloride-containing medium as an example. For example, the pitting corrosion process of stainless steel in a gas-filled chloride-containing medium: the metal surface in the pit is active.
The metal surface outside the corrosion hole is in a passive state and the potential is relatively positive, so an active-passive microgalvanic corrosion battery is formed inside and outside the hole, and the battery has a large cathode-small anode area Compared with the structure, the anode current density is very large, and the corrosion hole deepens rapidly. At the same time, the metal surface outside the hole is protected by cathodic protection, which can continue to maintain the passive state. The anodic dissolution reaction mainly occurs in the pore: Fe→Fe2++2e Cr→Cr3++3e Ni→Ni2++2e The main reaction outside the pore under neutral or weak alkaline conditions: 1/2 O2+H2O+2e →2OH-
The cathode and anode are separated from each other, and the secondary corrosion products will be formed in the orifice without much protection. The medium in the pores is in a stagnant state relative to the medium outside the pores, and the dissolved metal cations are not easy to diffuse out, and the dissolved oxygen is not easy to diffuse in. Due to the increase in the concentration of metal cations in the pores, the negatively charged chloride ions migrate into the pores to maintain electrical neutrality, and a concentrated solution of metal chlorides (such as FeCl2, etc.) is formed in the pores.
The metal surface in the pores continues to maintain activity. In addition, due to chloride hydrolysis and other reasons, the acidity of the medium in the pores increases, which further accelerates the dissolution rate of the anode. In addition, due to the action of gravity, the corrosion pores accelerate to develop deeper.